It occurs when laminating overlaminate to print. It is very noticeable in the dark shadow area of the print.
Silvering occurs when tiny air bubbles are captured between adhesive and ink:
In general, the overlaminate adhesive will wet out in 12-24 hours on water-based, eco-solvent, solvent, and latex ink. With the same clear overlaminate, moderate to heavy silvering will initially occur on UV ink. Even with adhesive wet out, silvering may still occur due to highly uneven UV ink surface.
Silvering usually does not occur on Eco-Solvent ink or it wet out in 24 hours:
Silvering does not occur on Latex ink or it wet out in 24 hours:
Silvering occurs on UV ink becuase of the uneven ink surface:
Today, there are many UV inks on the market, each with distinctive levels of smoothness and surface energy which contribute to overlaminate silvering and lifting. UV inks with a smoother topography and higher surface energy are more ideal for overlaminate compatibility. It is highly recommended to perform peel adhesion tests and silvering analysis of the overlaminate on the UV ink before beginning production. Even though silvering occurs on UV inks, overlaminates may still adhere well.
Heat assistant may help minimize the amount of silvering. Recommended settings for hot roll lamination:
The hot roll lamination guideline is based on the result obtained from a test laminator model. Your laminator model may require a different setting. Arlon makes no warranties on silvering improvement for hot roll lamination due to UV ink topography.